Inconel Alloy X-750 is a nickel-chromium austenitic alloy similar to Alloy 600 but made precipitation-hardenable by additions of aluminum and titanium. It has good resistance to corrosion and oxidation along with high tensile and creep-rupture properties at high temperatures to 1300°F (700°C). Extended applications that require high strength at temperatures beyond 1100°F (593°C) may require a solution treatment, with air cooling between intermediate and final aging.
Nickel Alloy X-750 displays excellent workability including machinability and welding. It is precipitation hardenable. This material has excellent relaxation resistance and is non-magnetic. It has enhanced elevated temperature strength properties to 1300ºF (700°C) and oxidation resistance to 1800ºF (983˚C). Inconel X-750 is resistant to a wide variety of industrial corrosives under both oxidizing and reducing conditions. This alloy also has excellent resistance to chloride stress corrosion cracking in the fully age hardened condition.
Weight % | Ni +(Co) | Cr | Fe | Ti | Al | Nb + (Ta) | Mn | Si | S | Cu | C | Co |
X-750 UNS N07750 |
70 min | 14-17 | 5-9 | 2.25-2.75 | 0.40-1.0 | 0.70-1.2 | 1 max | 0.50 max | 0.01 max | 0.50 max | 0.08 max | 1 max |
Grade | UNS | DIN | EN | AMS | ASTM | JIS | |
Inconel X-750 | N07750 |
2.4669 |
AMS 5598 AMS 5542 |
ASTM B637 |
- |
Rod | Bar | Forging Stock | Plate | Sheet | Strip | Wire |
ASTM B637 AMS 5667 AMS 5668 AMS 5669 AMS 5670 AMS 5671 AMS 5747 |
ASTM B637 AMS 5667 AMS 5668 AMS 5669 AMS 5670 AMS 5671 AMS 5747 |
ASTM B637 AMS 5667 AMS 5668 AMS 5669 AMS 5670 AMS 5671 AMS 5747 |
AMS 5542 AMS 5598 |
AMS 5542 AMS 5598 |
AMS 5542 AMS 5598 |
AMS 5698, AMS 5699 |
Property | 20°C | 200°C | 400°C | 427 °C | 538 °C | 600°C | 649°C | 732°C | 816°C |
Ultimate Tensile Strength /MPa | 1503.1 | 1351.4 | 744.6 | 688.8 | - | 622.6 | 593 | - | 600 |
0.2% Yield Strength /MPa | 979.1 | 737.7 | 365.4 | 340.6 | - | 278.5 | 250.3 | - | 253.7 |
Elongation % | 36 | 49 | 47 | 47 | - | 46 | 47 | - | 48 |
Charpy Impact V-notch /J | 436.6 | 115.2 | 189.8 | - | - | - | - | - | - |
Coefficient of Thermal Expansion µm/mC | - | - | - | 14.22 | 14.94 | 15.12 | 15.48 | 15.66 | 15.84 |
Thermal Conductivity /kcal/(hr.m.°C) | - | - | 10 | 11.2 | 12.1 | 12.9 | 15 | 15.66 | 15.84 |
Modulus of Elasticity / x105 MPa | - | - | 1.95 | 1.89 | - | 1.8 | 1.71 | - | 1.61 |